- Conditioning Fibreboards

Before final fixing fibreboards should be conditioned ie. bring their moisture content into equilibrium with their surroundings in order to help prevent subsequent movement problems.

BOARD TYPE CONDITIONING BY EXPOSURE TO AIR CONDITIONING WITH WATER
(in unheated buildings etc.)
Standard Hardboard 3 to 5 Days Ideally 48 to 72 Hrs - min 24Hrs
Tempered Hardboard 5 to 7 Days Ideally 72 to 96 Hrs - min 24Hrs
Medium Density Fibreboard (MDF) Only required if boardshave become very dry, 3 Days Not Recommended
Insulating Boards Remove all packaging, I to 2 Days Not Recommended
Flame Retardant Board FR Boards contain water soluble salts so must always be conditioned in air Not Recommended

To condition with water lay the boards down under cover. With a brush, rub clean water into the back face of the board at the rate of half to one litre for a board 2440 x 1220 x 3.2mm. Work from the centre outwards then place them wet side to wet side in a neat stack. The boards should then be allowed to stand for the appropriate minimum length of time given above.